C max |
Si max |
Mn | P max |
S max |
N max |
Addition of Nitrogen combining elements | Cr | Cu |
0.13 |
0.40 |
0.20-0.60 | 0.035 |
0.030 |
- |
yes | 0.40-0.80 | 0.25-0.55 |
Grade |
Mechanical Property |
|
|||
Tensile Strength(MPa) |
Yield Strength(MPa) |
% Elongation in 2 in.(50mm) min |
Impacting Test Temperature(°C) |
|
|
EN10025-5 S235J2W |
360 |
235 |
17 |
-20 |
|