UNE36011 C45K steel plate high carbon steel
C45K is a medium carbon steel is used when greater strength and hardness is desired than in the "as rolled" condition. Extreme size accuracy, straightness and concentricity combine to minimize wear in high speed applications. Turned, ground and polished.
UNE 36011 C45K steel Applications
Quenched and subsequently tempered steel for screws, forgings, wheel tyres, shafts, sickles, axes, knives, wood working drills, hammers, etc.
C45K UNE 36011 Number:1.0503 | Comparision of steel grades | |
JIS G 4051 | S 45 C | |
DIN 17200 | C 45 | |
NFA 33-101 | AF65-C 45 | |
UNI 7846 | C 45 | |
BS 970 | 070 M 46 | |
EN 10083-2 | C 45 | |
SAE J 403-AISI | 1042/1045 |
UNE 36011 C45K steel Chemical Composition
Grade | C(%)min-max | Si(%)min-max | Mn(%)min-max | P(%)max | S(%)max | Cr(%)min-max |
C45K | 0.42-0.50 | 0.15-0.35 | 0.50-0.80 | 0.025 | 0.025 | 0.20-0.40 |
UNE 36011 C45K steel Mechanical Properties
Grade | Condition | Yield Strength R°(Mpa) | Tensile Strength Rm (Mpa) | Elon- gation A5(%) | Hardness HRC | Quenching Temperature (℃) | Benda- bility | Nominal Thickness,t 1.95mm≤t≤10.0mm | |
Rolled | Annealed | ||||||||
C45K | Rolled Annealed Water-quenched Oil quenched | 460 330 | 750 540 2270 1980 | 18 30 | 58 55 | 820 860 | Min.reco-mmended Bending radius (≤90°) | 2.0 ×t | 1.0×t |