JIS G4303 SUS 416 Stainless steel
SUS 416 stainless steel has the highest machinability of any stainless steel, at about 85% of that of a free-machining carbon steel. As for most other free-machining stainless steels the improvement in machinability is achieved by addition of sulphur which forms manganese sulphide inclusions; this sulphur addition also lowers the corrosion resistance, weldability and formability to below that of its non-free machining equivalent 410 stainless steel.
SUS 416 stainless steel chemical composition:
Grade |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
N |
|
416 |
min. |
- |
- |
- |
- |
0.15 |
12.0 |
- |
- |
- |
SUS 416 stainless steel mechanical property:
Tempering Temperature (°C) |
Tensile Strength (MPa) |
Yield Strength |
Elongation |
Hardness Brinell |
Impact Charpy V (J) |
Annealed * |
517 |
276 |
30 |
262 |
- |
Condition T ** |
758 |
586 |
18 |
248-302 |
- |
204 |
1340 |
1050 |
11 |
388 |
20 |
316 |
1350 |
1060 |
12 |
388 |
22 |
427 |
1405 |
1110 |
11 |
401 |
# |
538 |
1000 |
795 |
13 |
321 |
# |
593 |
840 |
705 |
19 |
248 |
27 |
650 |
750 |
575 |
20 |
223 |
38 |
SUS 416 stainless steel physical property:
Grade |
Density (kg/m3) |
Elastic Modulus (GPa) |
Mean Coefficient of Thermal Expansion |
Thermal Conductivity |
Specific Heat 0-100°C |
Electrical Resistivity (nW.m) |
|||
0-100°C |
0-315°C |
0-538°C |
at 100°C |
at 500°C |
|||||
410 |
7750 |
200 |
9.9 |
11.0 |
11.6 |
24.9 |
28.7 |
460 |
570 |