JIS G4303 SUS 347 Stainless steel
Similar to 321 stainless steel, SUS 347 stainless steel uses columbium as a stabilizing element to maximize its principal feature: resistance to intergranular corrosion. SUS 347 stainless steel can be used in applications requiring repeated heating in the range of 800 and 1650 F (427-899 C).
SUS 347 stainless steel chemical composition:
Carbon 0.08 max
Chromium 17 - 19
Iron Balance
Manganese 2 max
Nickel 9 - 13
Niobium Min:10 x C
Phosphorus 0.045 max
Silicon 1 max
Sulphur 0.03 max
SUS 347 stainless steel physical property:
Density (lb / cu. in.) 0.29
Specific Gravity 8.03
Specific Heat (Btu/lb/Deg F - [32-212 Deg F]) 0.12
Electrical Resistivity (microhm-cm (at 68 Deg F)) 438
Melting Point (Deg F) 2600
Modulus of Elasticity Tension 28
To serve the interest and the needs of the public, as well as of our clients, BEBON STEEL will hold the belief "product quality and service foremost, sincerity and superior quality" forever. So if interest in SUS 347 stainless steel, pleace contact BEBON STEEL.