Under A131 rule, A131 E32 steel,A131 E36 steel and A131 E40 steel high strength steel plates shall be under the TMCP
or Normalized delivery condition. EH Class shall be done the low temperature impacting test at -40℃ with minimum impact energy 34 J longitudinally.For getting a better property of plates,our engineers
suggest customers do Z-Test for the thickness above 40mm,inculding Z15,Z25 and Z35.
A131 |
||||||
Grade |
ABS E32 |
ABS E36 |
ABS E40 |
|||
Chemical Composition % ≤ |
C |
0.18 |
||||
Mn |
0.90-1.60 |
|||||
Si |
0.10-0.50 |
|||||
P |
0.035 |
|||||
S |
0.035 |
|||||
Al (acid) |
0.015 |
|||||
Nb |
0.02-0.05 |
|||||
V |
0.05-0.10 |
|||||
Ti |
0.02 |
|||||
Cu |
0.35 |
|||||
Cr |
0.20 |
|||||
Ni |
0.40 |
|||||
Mo |
0.08 |
|||||
N |
- |
|||||
Mechanical Property ≥ |
Yield Strength (Mpa) |
315 |
355 |
390 |
||
Tensile Strength (Mpa) |
440-590 |
490-620 |
510-650 |
BEBON A131 E32 steel,A131 E36 steel and A131 E40 steel shipbuilding steel plates and sheets have been exported to worldwide shipyard and ship building company,we have mill A131 E32,A131 E36 and A131 E40 for shipbuilding.If you have any needs in A131 Grade DH32 DH36 DH40 steel plate price and suppliers, please feel free to contact us.
TAG:A131 E32 steel,A131 E36 steel and A131 E40 steel
Source:
Tags: