P275NH WSt285 A42CP AP FP
P275NHEN 10028-2 | Comparison of steel grades | |
EU 113 | - | |
NBN629> | - | |
DIN 17135 | WSt 285 | |
NFA36205 | A 42 CP,AP,FP |
Chemical Composition
Grades | C max | Si max | Mn. max | P max | S max | max | AL min | Cr max | Cu max | Mo max | Ni max | Nb max | Ti max | V max |
P275NH | 0.16 | 0.40 | 0.80-1.50 | 0.025 | 0.015 | 0.012 | 0.020 | 0.300 | 0.30 | 0.08 | 0.50 | 0.05 | 0.03 | 0.05 |
MechanicalPropertities
Grade | Thickness ( mm) | Yield Strength MPa(min) |
Tensile Strength MPa |
Elongation % (min) |
P275NH | ≤ 16 | 275 | 390 to 510 | 24 |
16<t ≤40 | 265 | 390 to 510 | 24 | |
40<t ≤60 | 255 | 390 to 510 | 24 | |
6<t ≤100 | 235 | 370 to 490 | 23 | |
100<t ≤150 | 225 | 360 to 480 | 23 | |
150<t ≤250 | 215 | 350 470 | 23 |
Source:
Tags: