EN10028-2 standard specification for non-alloy and alloy steels with specified elevated temperature properties. It covers steel grade P235GH, P265GH, P295GH, P355GH, 16Mo3, 18MnMo4-5, 20MnMoNi4-5, 15NiCuMoNb5-6-4, 13CrMo4-5, 13CrMoSi5-5, 10CrMo9-10, 12CrMo9-10, X12CrMo5, 13CrMoV9-10, 12CrMoV12-10, X10CrMoVNb9-1.
Bebon International specializes in the above steel plates comply with EN10028-2. We are assure of supplying 12CrMo9-10 in superior quality. The maximum thickness can reach 400mm.
If need more detail information of 12CrMo9-10 steel plate, please check the following:
EN10028-2 12CrMo9-10 steel Chemical Composition:
Chemical Composition of 12CrMo9-10, cast analysis |
||||||
Grade |
The Element Max (%) |
|||||
C |
Si |
Mn |
P |
S |
Al(min) |
|
12CrMo9-10 |
0.10-0.15 |
0.30 |
0.3-0.80 |
0.015 |
0.010 |
0.01-0.040 |
Cr |
Cu |
Mo |
Nb |
Ni |
Ti |
|
2.0-2.5 |
0.25 |
0.9-1.10 |
|
0.30 |
|
EN10028-2 12CrMo9-10 steel Mechanical Properties:
Mechanical Properties of 12CrMo9-10 at ambient temperature |
||||||
Grade |
Thickness |
Yield |
Tensile Strength |
Elongation |
Charpy V Notch Impact Test |
|
Degree |
Min Value |
|||||
12CrMo9-10 |
mm |
Min Mpa |
Mpa |
Min % |
℃ |
J |
5≤t≤250 |
355 |
540-690 |
18 |
-20 |
27 |
|
Note: Impact energy for impact test is on longitudinal |
EN10028-2 12CrMo9-10 steel Supplementary requirements:
1. Simulated Post Weld Heat Treatment of Mechanical Test Coupons (PWHT)
2. Drop Weight Test
3. High Temperature Tension Test
4. Ultrasonic Examination in EN10160-(S3E3/S3E4,S2E2/S2E3,S1E1/S0E1), SEL072-Ⅰ/Ⅱ/Ⅲ/Ⅳ, A435/A435M, ASTM A578 Level A/B/C
5. Z15, Z25, Z35 test
6. Hydrogen sulfide resistant test: HIC test comply with NACE TM0284; CLR≤15%, CTR≤5%, CSR≤1.5%; SSCC test shall be carried out as per NACE MR0175/ISO 15156.