Conditions for heat treating test bars and treatment of the steels
End quenchh test
Quenching, 0C
|
Carbunnzing temperature, 0C
|
Core-hardening temperature, 0C
|
Case-hardening temperature, 0C
|
Tempering, 0C
|
910
|
880 to 980
|
860 to 900
|
780 to 820
|
150 to 200
|