Designation
|
Min. Yield
Strength ReH2) [MPa] |
Tensile
Strength Rm [MPa] |
Min. Elongation
[%] |
Min. Impact
Energy KV [°C/J] - longitudinal |
CEV max.1)
|
Dimension
Table No. |
Max.
Thickness [mm] |
Max. Thickness
for option (C) [mm] |
S235JR(C)
|
235
|
360-510
|
24
|
+20/27
|
0,35
|
Table 1
|
80 3)
|
30 4)
|
S235J0(C)
|
235
|
360-510
|
24
|
0/27
|
0,35
|
Table 1
|
80 3)
|
30 4)
|
S235J2(C)
|
235
|
360-510
|
24
|
-20/27
|
0,35
|
Table 1
|
80 3)
|
30 4)
|
S275JR(C)
|
275
|
410-560
|
21
|
+20/27
|
0,40
|
Table 1
|
80 3)
|
30 4)
|
S275J0(C)
|
275
|
410-560
|
21
|
0/27
|
0,40
|
Table 1
|
80 3)
|
30 4)
|
S275J2(C)
|
275
|
410-560
|
21
|
-20/27
|
0,40
|
Table 1
|
80 3)
|
30 4)
|
S355JR(C)
|
355
|
470-630
|
20
|
+20/27
|
0,45
|
Table 1
|
80 3)
|
30 4)
|
S355J0(C)
|
355
|
470-630
|
20
|
0/27
|
0,45
|
Table 1
|
80 3)
|
30 4)
|
S355J2(C)
|
355
|
470-630
|
20
|
-20/27
|
0,45
|
Table 1
|
80 3)
|
30 4)
|
1) CEV= ; valid for thickness up to 30 mm, for higher thickness refer to the standard
EN 10025+A1
|
DIN 17100
|
BS 4360
|
NFA 35-501
|
|
S235JR(C)
|
S235JRG2(C)
|
RSt 37 - 2
|
40 B
|
E 24 - 2
|
S235J0(C)
|
S235J0(C)
|
St 37 - 3U
|
40 C
|
E 24 - 3
|
S235J2(C)
|
S235J2G4(C)
|
St 37 - 3N
|
40 D
|
E 24 - 4
|
S275JR(C)
|
S275JR(C)
|
St 44 - 2
|
43 B
|
E 28 - 2
|
S275J0(C)
|
S275J0(C)
|
St 44 - 3U
|
43 C
|
E 28 - 3
|
S275J2(C)
|
S275J2G4(C)
|
43 D
|
E 28 - 4
|
|
S355JR(C)
|
S355JR(C)
|
-
|
50 B
|
E 36 - 2
|
S355J0(C)
|
S355J0(C)
|
St 52 - 3U
|
50 C
|
E 36 - 3
|
S355J2(C)
|
S355J2G4(C)
|
St 52 - 3N
|
50 D
|
-
|
S355K2(C)
|
S355K2G4(C)
|
-
|
50 DD
|
E 36 - 4
|
Source:
Tags: en10025 s235jr, s235j0, s235j2, s275jr, s275j0, s275j2, s355jr, s355j0, s355j2, s235jr, s235j0, s235j2, s275jr, s275j0, s275j2, s355jr, s355j0, s355j2 steel plate.