A 588 Gr B welding procedure, A 588 Gr B applications

A 588 Gr B welding procedure, A 588 Gr B applications

A 588 Gr B welding procedure, A 588 Gr B applications

by inspection on welded property and analysis on carton equivalent, the possibility of the quenching and cold crack of A 588 Gr B steel is small, so it can welded without preheat.
According to the ASTM A 588 Gr B chemical composition, ASTM A 588 Gr B mechanical property,  A 588 Gr B characteristics, A 588 Gr B applications.

A 588 Gr B has wide applications:
A588 Gr B steel plate, this kind of steel is not easy to rust. when steel plate were exposed in the atmosphere, Cu and P were combined into a dense layer of Oxidation film, and Cr and Ni also can make an Oxidation film, so the kind of steel has a very good corrosion resistant.
A 588 Gr B steel was widely used in railway, vehicle, bridgh, tower structure, other steel structure and container, oil cylinder, chimney, curtain wall, outdoor sculptures, etc, which are exposed in atmosphere for long time.

If you want to know more about A 588 Gr B welding procedure, A 588 Gr B applications, welcome to contact our sale team, our professional sales team will answer you within 24 hours.

Besides, we also supply A 588 Gr B steel service:
Pretreatment(Derusting,Lacquering,Painting,Sand Clusting),Heat treatment,UT Test,HIC Test,Impact Test,PWHT Z15 Test, Z25 Test, Z35Test,Cutting, Welding ,Inspection from the third party like SGS,Galvanization

A588 Grade B steel delivery conditions:
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.we also can supply weathering resistant steel of S235J2W Steel , S355J0WP Steel , S355J2G1W Steel , S355J2G2W Steel,please contact us if you need.

Source:

Tags:

Related Products
ADD:Headquarters Enterprise Base, Ruida Road,
Zhongyuan District, Zhengzhou City, 450000,China
TEL: 0086-371-86151827 ,0086-371-86151527
FAX: 0086-371-86011881
E-MAIL: [email protected]
Website : www.bebonchina.com
MESSAGE