24 Hour Emergency Steel Machining Response
OR
Home > steel coil > shipbuilding steel coil > EN10225

EN10225 S355G2+N Shipbuilding Steel Coil

EN10225 S355G2+N Shipbuilding Steel Coil Chemical Composition and Mechanical Property

C max Si max. Mn P max S max Cr max. Mo max. Ni max. Al min. Cu max. N max. Nb max. Ti max. V max. Cr+Mo+Ni+ Cu max. Nb+V max. Nb+V+Ti max.

0.20

0.50 0.90-1.65

0.035

0.030

0.30 0.10 0.05 0.02 0.35 0.015 0.060 0.030 0.12 - ]

-

Yield Strength (MPa) min. (t≤16mm) Yield Strength (MPa) min. (16<t≤25mm) Yield Strength (MPa) min. Elongation min. %
355 345 470-630 22

EN10225 S355G2+N Shipbuilding Steel Coil Application

EN10225 S355G2+N shipbuilding steel, EN10225 S355G2+N shipbuilding steel coil

EN10225 S355G2+N Shipbuilding Steel Coil Other Name

EN10225 S355G2+N shipbuilding steel, EN10225 S355G2+N shipbuilding steel coil

Additional Condition

UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.

Other Terms

Packaging Details: Standard export seaworthy packing or as required.
Delivery Time: 30-50 days, 7 days for stock goods.
Loading Port: Shanghai ,Tianjin, Qingdao.
Offer Ability:5 000MT/Per Month.
MOQ: 1 Pcs.