24 Hour Emergency Steel Machining Response
OR
Home > steel coil > Pipeline Steel Coil > API 5CT-2011

API 5CT-2011 K55 Pipeline Steel Coil

API 5CT-2011 K55 Pipeline Steel Coil Chemical Composition and Mechanical Property

C

Si

Mn

P

S

Cr

Ni

Cu

Mo

V

Als

0.34~0.39

0.20~0.35

1.25~1.50

≤0.020

≤0.015

≤0.15

≤0.20

≤0.20

   

≤0.020

Steel Grade Yield Strength (Mpa) Tensile Strength (Mpa)
API 5CT J55

≥655

≥655

API 5CT-2011 K55 Pipeline Steel Coil Application

API 5CT-2011 K55 pipeline steel coil is used in Oil and Gas Project.

API 5CT-2011 K55 Pipeline Steel Coil Other Name

API 5CT-2011 pipeline steel coil, API 5CT K55 pipeline steel coil

Additional Condition

UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.

Other Terms

Packaging Details: Standard export seaworthy packing or as required.
Delivery Time: 30-50 days, 7 days for stock goods.
Loading Port: Shanghai ,Tianjin, Qingdao.
Offer Ability:5 000MT/Per Month.
MOQ: 1 Pcs.